Zinc Cathodes

Service life≥12 Months

A00 Cathodes

Back

Zinc CathodesOverview of

The cathode plate for zinc electrodeposition is composed of such parts as aluminum plate, aluminum alloy conducting beam or pure aluminum conducting beam, composite conducting head (conducting strip), and lifting lugs and process by a specific process to be suitable for hydrometallurgical zinc electrodeposition.

Parameter Information

Some Patented Technology Products

Three-side Injection Molding

A high-pressure injection molding process is performed at the cathode plate edges, and the insulation strips on the three sides are formed in one piece, which is not easy to fall off and has a long service life.

Coating

High-polymer strong plastic corrosion-resistant materials are used and a special process is applied to protect the cathode plate liquid level from corrosion. The insulation strips on the three sides are formed integrally by high-pressure injection molding process and are not easy to fall off.

Rubber vulcanization

Modified rubber vulcanization materials and a cladding process are used to form the cathode plate edge and liquid level protection position integrally, thus forming the overall insulation protection of the plate, strong adhesion of the materials and long service life of the plate.